Thermal Properties Metric English Comments
Pour Point 10.0 °C
50.0 °F
Base Oil; ASTM D97
Nye Lubricants 439 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point 10.0 °C
50.0 °F
Base Oil; ASTM D97
Nye Lubricants 520C-2 (NT) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point 10.0 °C
50.0 °F
Base Oil; ASTM D97
Nye Lubricants 520M-2 (NT) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point 10.0 °C
50.0 °F
Base Oil; ASTM D97
Nye Lubricants 520M-2-UV (NT) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point 10.0 °C
50.0 °F
Base Oil; ASTM D97
Nye Lubricants 523V-2-UV (NT) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point 10.0 °C
50.0 °F
Solvay ALKAMULS® EL 620 LI E Surfactant
Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Identification: CASTOR OIL ETHOXYLATE (30)CAS: 61791 – 12 â€..
Pour Point 10.0 °C
50.0 °F
Solvay ALKAMULS® EL 719 E Surfactant
Identification: ETHOXYLATED CASTOR OILCAS: 61791 – 12 – 6Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North Ameri..
Pour Point 10.0 °C
50.0 °F
ASTM D97
ChevronTexaco 800 NC Open Gear Lubricant
FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri..
Pour Point 10.0 °C
50.0 °F
ChevronTexaco Sugartex® Heavy
Texaco Sugartex delivers value through:Reliability — High lubricant film strength withstands heavy shock loads and provides protection under boundary lubrication to minimize wear rate and prevent f..
Pour Point 10.0 °C
50.0 °F
ConocoPhillips Inca® 1000 Oil, AGMA No. 8A Comp.
Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures..
Pour Point 10.0 °C
50.0 °F
ChevronTexaco Sugartex®
Texaco Sugartex delivers value through:Reliability — High lubricant film strength withstands heavy shock loads and provides protection under boundary lubrication to minimize wear rate and prevent f..
Pour Point 10.0 °C
50.0 °F
Solvay LUBRHOPHOS® RD 510 E Surfactant
Identification: POLYOXYETHYLENE LAURYL ETHER PHOSPHATECAS: 39464 – 66 – 9Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin Ame..
Pour Point 10.0 °C
50.0 °F
Solvay RHODASURF® CET 5 Surfactant
Identification: ETHOXYLATED OLEYL CETYL ALCOHOLCAS: 68920 – 66 – 1Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America an..