Polymer Property : Pour Point = -60.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point -51.1 °C
-60.0 °F
Lubriplate SFGO Ultra-150 PAO-Based Synthetic Food Machinery Grade Fluid
Polyalphaolefin (PAO)-based high-performance fluids formulated with 100% PAO synthetic base fluids for a variety of demanding applications. They are outstanding lubricants for use under severe condi..
Pour Point -51.1 °C
-60.0 °F
Lubriplate SYN LUBE 150 PAO-Based Multi-Purpose Synthetic Fluid
PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 150, 220, 320, 460 & 680 are recommended..
Pour Point -51.1 °C
-60.0 °F
Lubriplate SYN LUBE 68 PAO-Based Multi-Purpose Synthetic Fluid
PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 22, 32, 46, 68 & 100 are recommended for..
Pour Point -51.1 °C
-60.0 °F
Lubriplate NO.0 Petroleum-Based Machine Tool Oil
Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles..
Pour Point -51.1 °C
-60.0 °F
Lubriplate RCO 68 PAO-Based Synthetic Food Machinery Grade Fluid
Formulated for use in refrigeration compressor systems where a NSF H-1 Registered, food machinery grade lubricant is required.RCO-68 Fluid is available in Pails & Drums.H-1 Class Lubricants are manu..
Pour Point -51.1 °C
-60.0 °F
Lubriplate SFGO Ultra-68 PAO-Based Synthetic Food Machinery Grade Fluid
Polyalphaolefin (PAO)-based high-performance fluids formulated with 100% PAO synthetic base fluids for a variety of demanding applications. They are outstanding lubricants for use under severe condi..
Pour Point -51.1 °C
-60.0 °F
Lubriplate SYNCOOL 32 Polyglycolester-Based Synthetic Air Compressor Fluid
These polyglycolester-based synthetic fluids are designed for rotary screw air compressors. They offer excellent heat transfer properties, low evaporation, high flash points, and outstanding oxidati..
Pour Point -51.1 °C
-60.0 °F
ConocoPhillips Syncon® 32 Synthetic R&O Oil
Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv..
Pour Point -51.1 °C
-60.0 °F
ASTM D-97
ConocoPhillips ANDEROL® 783-0 Series Synthetic Food Grade Greases, NLGI Grade 0
Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases..
Pour Point -51.1 °C
-60.0 °F
ASTM D-97
ConocoPhillips ANDEROL® 783-00 Series Synthetic Food Grade Greases, NLGI Grade 00
Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases..
Pour Point -51.1 °C
-60.0 °F
ASTM D-97
ConocoPhillips ANDEROL® 783-1 Series Synthetic Food Grade Greases, NLGI Grade 1
Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases..
Pour Point -51.1 °C
-60.0 °F
ConocoPhillips Hydroclear® Automatic Transmission Fluid
Description: Conoco Hydroclear DEXRON® III & MERCON® Automatic Transmission Fluid is a multipurpose fluid for the electronically controlled transmissions of most domestic and imported automobiles,..