Polymer Property : Pour Point = -56.2 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point -49.0 °C
-56.2 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8140 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -49.0 °C
-56.2 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8160 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -49.0 °C
-56.2 °F
ASTM D97
Solvay Specialty Polymers FOMBLIN® LC80 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..
Pour Point -49.0 °C
-56.2 °F
Base Oil; ASTM D97
Nye Lubricants 344 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -49.0 °C
-56.2 °F
BASF Palatinol® N Diisononyl Phthalate
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl..
Pour Point -49.0 °C
-56.2 °F
PolyOne Synplast™ DINP-N Di Isononyl Phthalate
Branched C9 phthalate esterInformation provided by PolyOne