Thermal Properties Metric English Comments
UL RTI, Electrical 260 °C
500 °F
UL 746B
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
UL RTI, Electrical 260 °C
500 °F
UL 746B
Victrex® PEEK 450G General Purpose
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac..
UL RTI, Electrical 260 °C
500 °F
UL746B
Victrex® Vicote® 702 Polyetheretherketone (PEEK) Powder
Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail..
UL RTI, Electrical 260 °C
500 °F
UL 746B
Victrex® Vicote® 705 Black Polyetheretherketone (PEEK) Powder Coating
VICOTE 705Blk is a black pigmented version of the 705 grade. This grade has a nominal particle size of about 50 microns. The powder is dark grey in colour and is a low melt viscosity grade for low..
UL RTI, Electrical 260 °C
500 °F
UL746B
Victrex® Vicote® 709 Polyetheretherketone (PEEK) Powder
Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, ..
UL RTI, Electrical 260 °C
500 °F
UL746B
Victrex® Vicote® 708 Polyetheretherketone (PEEK) Powder
VICOTE 708 and 709 grades are specially developed powder coatings (based on VICTREX HT™ polymer) with a higher Tg and melting point than the standard VICOTE products. VICOTE 708 and 709 grades deli..
UL RTI, Electrical 260 °C
500 °F
UL746B
Victrex® Vicote® 706 Polyetheretherketone (PEEK) Powder
Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail..
UL RTI, Electrical 260 °C
500 °F
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
UL RTI, Electrical 260 °C
500 °F
UL 746B
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..
UL RTI, Electrical 260 °C
500 °F
UL746B
Victrex® Vicote® 701 Polyetheretherketone (PEEK) Powder
Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail..
UL RTI, Electrical 260 °C
500 °F
UL746B
Victrex® Vicote® 703 Polyetheretherketone (PEEK) Powder
Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail..
UL RTI, Electrical 260 °C
500 °F
UL746B
Victrex® Vicote® 704 Polyetheretherketone (PEEK) Powder
Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, ..
UL RTI, Electrical 260 °C
500 °F
UL 746B
Victrex® Vicote® 705 Blue Polyetheretherketone (PEEK) Powder Coating
VICOTE 705 Blue is a blue pigmented version of the VICOTE 705 grade and contains additives to help with adhesion, wetting of the substrate and shrinkage. This grade has a nominal particle size of ~ ..
UL RTI, Electrical 260 °C
500 °F
UL746B
Victrex® Vicote® 705 Polyetheretherketone (PEEK) Powder
Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail..
UL RTI, Electrical 260 °C
500 °F
UL746B
Victrex® Vicote® 707 Polyetheretherketone (PEEK) Powder
Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail..