Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
RheTech Products P256-762 Polypropylene Copolymer, Medium Grey Applications: Misc. ClipsElectrical housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® GP74G20 ABS, 20% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed (0.250 in); ASTM D648 |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed; ASTM D648 |
LyondellBasell Pro-faxâ„¢ SG899 Polypropylene Copolymer Description: Pro-faxâ„¢ SG899 high flow, high impact polypropylene copolymer resin is tailored for use in automotive interior head impact applications. This resin is designed to be run in convent.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed; ASTM D648 |
M. Holland Company RP200 Polypropylene Copolymer Features: High ClarityUses: Bottles, Food Containers Approvals: FDA 21 CFR 177.1520Processing Method: Extrusion Blow Molding, Injection Blow MoldingInformation provided by M. Holland. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed; ASTM D648 |
Global PP-2300-K Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed; ASTM D648 |
Global PP-2300-LC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed; ASTM D648 |
Global PP-2300-NC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed; ASTM D648 |
Teknor Apex Sinelec CCB1834 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Forms: Pellets Processing Method: Injection MethodInformation Provided by Teknor Apex.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ISO 75-2/B |
ExxonMobil Exxtral™ BMU 141 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive instrument panels in which good surface finish, high s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Clariant 6008 L Nylon 6, High Impact, Injection Molding Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accucomp ABS ABS892BL High Heat Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accutech ABS ABS833G10L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437T20L1 Talc Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437W30L1 Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0336C10L1 Calcium Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Americas Styrenics MB3150 High Heat Crystal Polystyrene Product CharacteristicsFast cycling due to high heat distortion temperatureHigh vicat softening temperatureExcellent clarity with slight blue tintGood toughnessFood Contact CompliantUL Classificatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Americas Styrenics STYRON® 686E High Heat Crystal Polystyrene Product CharacteristicsExceptional balance between heat resistance, toughness and flowGood dimensional stability and excellent clarityFood Contact CompliantTypical ApplicationsFoamed PS sheets used .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accutech ABS ABS831G20L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Ineos H07B-00 Polypropylene Homopolymer This is a polypropylene homopolymer for cast film applications that require antiblock additives. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 17.. |