Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C @Treatment Temp. 50.0 °C, Thickness 3.18 mm |
171 °F @Treatment Temp. 122 °F, Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ L6105 natural Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 - 107 °C | 171 - 225 °F | Average value: 89.5 °C Grade Count:55 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C | 171 °F | Unannealed; ASTM D648 |
LyondellBasell Pro-faxâ„¢ SR257M Polypropylene Copolymer Description: Pro-faxâ„¢ SR257M clarified polypropylene random copolymer resin has excellent see-through and contact clarity. This resin offers source reduction potential in blow molding and extru.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C | 171 °F | ASTM D648 |
Ineos T50-800-01 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C | 171 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hifaxâ„¢ CB276 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB276 very high melt flow, 1,200 MPa flexural modulus, UV-stabilized, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C | 171 °F | Unannealed; ISO 75-2/Bf |
Styron INSPIREâ„¢ T710-25 ES PolyPropylene Resin DA Thermoplastic Polyolefin Dow T710-25 ES Polypropylene Resin DAâ„¢ is a high impact TPO with enhanced flow, scratch and mar, and surface aesthetics for excellent molded-in-color appearance for automotive interior applicat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C | 171 °F | ISO 75-2/B |
ExxonMobil Exxtral™ CNR 012 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe South America and Nort.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C | 171 °F | ASTM D648 |
Aclo Accuguard ABS ABS860V0L Flame Retardant |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C | 171 °F | ASTM D648 |
Aclo Accuguard Polypropylene CP0467V2CSL Copolymer Flame Retardant Copper Stabilized |