Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C @Thickness 6.35 mm |
163 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Fittings M1000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C @Thickness 6.35 mm |
163 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Fittings M1005 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | ASTM D648 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | Unannealed; ASTM D648 |
Global PP-2800-J Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-automotive (interior & exterior), cratesInformation provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | ISO 75-2/B |
ExxonMobil Exxtral™ CNU 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications in which good surface finish and UV resistance is required. Availabilit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DMDA-8907 NT 7 High Density Polyethylene Resin DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DMDA-8920 NT 7 High Density Polyethylene Resin DOW DMDA-8920 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPE LD 300-1 Low Density Polyethylene Compounded Resin AAROLENE® ARPE 300 Series Polyethylene Compounded Resin LDPEColor may be specified. Melt Flow Index may be specified. Specific Gravity may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | ASTM D648 |
Aaron Industries AVPE LD 300-1 MELT 20 Virgin Polyethylene A natural, high flow Low Density Polyethylene resin, specifically designed for high speed injection molding applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | ASTM D648 |
Aaron Industries AVPE LD 300-1 Virgin Polyethylene Melt flow index may be specified. |