Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.2 - 143 °C
162 - 290 °F
Average value: 123 °C Grade Count:42
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
Ineos R01C-00 Polypropylene Random Copolymer
Grade R01C-00 is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding, through it is clarifier/antistat additive combination. Applications that requi..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® HDPE 8904 FR UV GY
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceAppearance: GrayInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
Unannealed; ASTM D648
Techmer ES HiFill® HDPE 8904 UV GY
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: GreyInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
Spartech Solarex® SV Copolyester Sheet
Description: Copolyester SheetInformation provided by Spartech.
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
unannealed (0.125 in); ASTM D648
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures ..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
ExxonMobil PP9513 Polypropylene Homopolymer
Product Description: A random copolymer resin designed for non-oriented film.Availability: North America Features:Controlled RheologyEthylene Oxide SterilizableUses: BagsCast FilmHeavy-duty BagsPac..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
Molded and tested in accordance with ASTM D4976; ASTM D648
Dow DMDA-8904 NT 7 High Density Polyethylene Resin
DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
Unannealed; ASTM D648
Dow R792-35RNA Polypropylene Random Copolymer Resin
OverviewControlled rheology productConsistent processabilityContains clarifying additiveContains an antistatic additiveComplies with U.S. FDA 21 CFR 177.1520 (c)3.1a, Canadian HPFB No ObjectionDOW R..
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
Aclo Accutech Polypropylene Copolymer CP0437C10L Calcium Reinforced
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
unannealed; ASTM D-648
Axiall 8607 Rigid PVC, Extrusion
Georgia Gulf 8607 is a special purpose pelletized compound formulated for high impact, rigid extrusion profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.