Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 301 °C

@Thickness 3.20 mm
574 °F

@Thickness 0.126 in
Annealed; ASTM D648
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Deflection Temperature at 0.46 MPa (66 psi) 301 °C

@Thickness 3.20 mm
574 °F

@Thickness 0.126 in
Annealed; ASTM D648
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha..
Deflection Temperature at 0.46 MPa (66 psi) 301 °C
574 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA
LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 301 °C

@Thickness 3.18 mm
574 °F

@Thickness 0.125 in
Annealed; ASTM D648
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0...