Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 527 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
Unannealed; ASTM D648
Multibase Nylex™ 2185 NAT Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
LATI Latigray 80-03 CWG/850 PPS, Glass/Metallic Reinforced
Radiopaque compound based on Polyphenylene Sulfide (PPS). Metallic filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by..
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Lubricomp OFG26XXP PPS - Linear
LNP* Lubricomp* OFG26XXP is a compound based on Linear PPS containing Glass Fiber and Graphite Powder. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for..
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear
LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber.
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP UCF22S PPA
LNP* Thermocomp* UCF22S is a compound based on Polyphthalamide resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive..
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear
LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Bf
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded
Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar.
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
ISO 75-1/-2
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Dry)  (discontinued **)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
LATI Laticonther 80 GR/50 PPS, 50% Graphite Reinforced
High thermal conductivity product based on Polyphenylene Sulfide (PPS). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
LATI Latilub 80-15T G/30 PPS, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOTUF OF008I PPS - Linear (Europe-Africa-Middle East)
LNP* Thermotuf* OF008I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact.