Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C @Thickness 6.35 mm |
480 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Therma-Tech™ NN-3000 TC Polyamide 66 (Nylon 66) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANAMID 66 A12^ F25 NH10 Nylon 66, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified Nylon 66, 13% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Polymer Resources NY66-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 CM40 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M25HS L BK 25% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight and Mineral Filler, 25% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON RX06001 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RX06001 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Easy Molding, High Impact, Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C @Thickness 3.20 mm |
480 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C @Thickness 3.20 mm |
480 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Clariant PA123G20 Nylon 66, 20% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Clariant Renol 6622-L Nylon 66, Glass Fiber Filled, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET 45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Adell AL-18 Nylon 66, 40% Glass Reinforced; Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Adell AL-38 Nylon 66, 40% Glass Reinforced; Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 249 °C | >= 480 °F | ASTM D648 |
Adell AR-38 Nylon 66, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Adell AT-37 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM Test |
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 7523-2AM BK ND3007 is an impact modified, 33% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Ashley Polymers Ashlene® 528LSB2-20G Nylon 66, 20% Glass Reinforced A UV Stabilized 20% glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 249 °C | >= 480 °F | ASTM D648 |
Adell AR-14 Nylon 66, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 249 °C | >= 480 °F | ASTM D648 |
Adell AR-17 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
Adell AT-34 Nylon 66, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |