Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 44.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont 20 Series 2020 Specialty Polyethylene Resin  (discontinued **)
DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium  (discontinued **)
Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C

@Thickness 3.20 mm
111 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 335 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C

@Thickness 3.20 mm
111 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 335 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont 20 Series 2010 Specialty Polyethylene Resin
DuPont 2010 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding fl..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont 20 Series 2020T Specialty Polyethylene Resin
DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont 20 Series 20-6064 Specialty Polyethylene Resin
DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont 20 Series DPE 20 Specialty Polyethylene Resin
DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C

@Thickness 3.20 mm
111 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 335 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C

@Thickness 3.20 mm
111 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 335 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C

@Thickness 3.20 mm
111 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 335 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C

@Thickness 3.20 mm
111 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 335 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium
Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont™ Surlyn® 8940 Ionomer Resin, Sodium
Surlyn® 8940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont™ Surlyn® 9910 Ionomer Resin, Zinc
Surlyn® 9910 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium
Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions ..
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
Spartech Spectrum® S630 MDPE Polyolefin Sheet  (discontinued **)
Data provided by the manufacturer.
Copyright © lookpolymers.com All Rights Reserved