Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C
102 °F
injection molded specimen; ASTM D648
Phillips Sumika Marlex® CHP-015 Thermoplastic Polyolefin  (discontinued **)
Applications: Driver-side air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 201..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C
102 °F
ASTM D648
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.17 mm
102 °F

@Thickness 0.125 in
ISO 75
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C
102 °F
ASTM D648
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.17 mm
102 °F

@Thickness 0.125 in
ISO 75
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C
102 °F
ASTM D648
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.17 mm
102 °F

@Thickness 0.125 in
ISO 75
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C
102 °F
ASTM D648
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C
102 °F
ASTM D648
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.17 mm
102 °F

@Thickness 0.125 in
ISO 75
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C
102 °F
ASTM D648
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.17 mm
102 °F

@Thickness 0.125 in
ISO 75
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.17 mm
102 °F

@Thickness 0.125 in
ISO 75
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C

@Thickness 3.20 mm
102 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..