Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 329 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 329 °C

@Thickness 3.20 mm
624 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK
LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 0.46 MPa (66 psi) 329 °C
624 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Deflection Temperature at 0.46 MPa (66 psi) 329 °C
624 °F
ISO 75
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion  (discontinued **)
AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil..