Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 318 °C
604 °F
Unannealed; ISO 75-2/B
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st..
Deflection Temperature at 0.46 MPa (66 psi) 318 °C
604 °F
HDT B; Unannealed; ISO 75-2/B
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig..