Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-00 13% Glass Fiber Reinforced Polypropylene, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-00UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-01 13% Glass Fiber Reinforced Polypropylene, Black Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-01UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-332UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 9772) Light Neutral Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-347UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, 109D Medium Pewter Applications: Dome lamp housingsFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-553UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 501F) Dark Smoke Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-589UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (YR169L) Mild Beige Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products G13P100-724UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, NH220L Clear Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 153 °C | 308 °F | ASTM D648 |
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products. |