Deflection Temperature at 0.46 MPa (66 psi) 151 °C
303 °F
ASTM D648
Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene
Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature..