Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 290 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in water-c..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ASTM D648
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded &a
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant
Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
LATI Laramid CE/60 PPA, 60% Mineral Reinforced
Semi-aromatic polyamide (PPA) based compound. Mineral filler. High dimensional stability. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP LCF62E PEEK
LNP* THERMOCOMP* LCF62E is a compound based on Polyetheretherketone resin containing 10% Carbon, 30% Glass Fiber fillers. Added features of this material includes: Easy Molding, Electrically Condu..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C

@Thickness 3.20 mm
554 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP LCF62E PEEK
LNP* THERMOCOMP* LCF62E is a compound based on Polyetheretherketone resin containing 10% Carbon, 30% Glass Fiber fillers. Added features of this material includes: Easy Molding, Electrically Condu..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
Average value: 290 °C Grade Count:16
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
ISO 75-1/-2
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Copyright © lookpolymers.com All Rights Reserved