Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 272 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched
LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific)
LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive..
Deflection Temperature at 0.46 MPa (66 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Thermocomp OF002A PPS
LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 0.46 MPa (66 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Thermocomp OF002A PPS (Asia Pacific)
LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.