Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 248 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 - 120 °C
219 - 248 °F
Reliance Industries Polypropylene Homopolymer
Typical properties of Reliance - Repol Polypropylene gradesInformation provided by Reliance Industries
Deflection Temperature at 0.46 MPa (66 psi) 75.0 - 120 °C
167 - 248 °F
Average value: 96.5 °C Grade Count:6
Overview of materials for PEN-PET
This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent..
Deflection Temperature at 0.46 MPa (66 psi) 110 - 120 °C
230 - 248 °F
ASTM D1525, HDT Method B
Loxim 500 00HB Polycarbonate/Acrylonitrile Butadiene Styrene
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 110 - 120 °C
230 - 248 °F
ASTM D1525, HDT Method B
Loxim 820 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 115 - 120 °C
239 - 248 °F
ASTM D1525, HDT Method B
Loxim 841 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 117 - 120 °C
243 - 248 °F
C.O.I.M. EXTER S® S 402 Isophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 402: High-quality re..