Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 87.8 - 190 °C | 190 - 374 °F | Average value: 133 °C Grade Count:41 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 - 190 °C | 176 - 374 °F | Average value: 102 °C Grade Count:34 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 175 - 190 °C | 347 - 374 °F | Average value: 181 °C Grade Count:5 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 187 - 190 °C | 369 - 374 °F | Average value: 188 °C Grade Count:3 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |