Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 86.7 °C | 188 °F | ASTM D648 |
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.7 °C | 188 °F | ASTM D648 |
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.7 °C | 188 °F | ASTM D648 |
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.7 °C | 188 °F | ASTM D648 |
Ineos H02G-02 Polypropylene Homopolymer This is a homopolymer designed for extrusion and film. It exhibits good extrusion and film orientation behavior. This material meets the requirements of the U.S. Food and Drug Administration as sp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.7 °C | 188 °F | ASTM D648 |
Ineos N00G-01 Polypropylene Impact Copolymer Grade N00G-01 is a fractional melt flow rate impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.7 °C | 188 °F | ASTM D648 |
Ineos N20L-00 Polypropylene Impact Copolymer This is a nucleated polypropylene impact copolymer formulated with a slip agent for improved mold release, and has an optimum balance of stiffness and impact resistance for injection molding applica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.7 °C | 188 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PP CO FR-N V2 Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.7 °C | 188 °F | ASTM D648 |
Plastics Group Polifil® RP-PP Polypropylene, Black Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low de.. |