Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
RheTech Products F49-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Fan shroudsSupport ductsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
RheTech Products GC30P100-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH GF5030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
Qualchem Danaprop PP2GF-15 Polypropylene, 15% Glass Fiber Polypropylene (homo-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C @Thickness 6.35 mm |
318 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Gravi-Tech™ GRV-NP-069-BMX Nylon 12
(discontinued **) |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
Kolon KOCETAL® K700BK Colored Grade Acetal Resin Colored, low viscosity grade.Applications: Thin products, improved appearance.Information provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C @Thickness 3.20 mm |
318 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP KB003RXZ Acetal Copolymer LNP THERMOCOMP* KB003RXZ is a compound based on Acetal Copolymer resin containing 15% Glass Bead. Added features of this material include: Easy Release. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ISO 75-2 |
Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ISO 75-2 |
Borealis GB366WG Polypropylene Compound, Glass Fiber Reinforced GB366WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ISO 75-2 |
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
Ecomass® 1700CO93 Copper Powder Filled Polyamide, Injection Molding High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | |
BASF Procom® GC30S 403 Polypropylene Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
A. Schulman ComAlloy Aqualoy® 125 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 112 Polypropylene, Glass Reinforced, Chemically Coupled, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
A. Schulman ComAlloy Voloy® 112 Polypropylene, Glass Reinforced, Chemically Coupled, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-35FM-1309 35% Glass and Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
RheTech Products GC30P100-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C @Thickness 3.20 mm |
318 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410 |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |