Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 70.0 - 107 °C | 158 - 225 °F | Average value: 94.4 °C Grade Count:36 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 - 107 °C | 171 - 225 °F | Average value: 89.5 °C Grade Count:55 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 - 107 °C | 185 - 225 °F | Average value: 97.1 °C Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.3 - 107 °C | 200 - 225 °F | Average value: 102 °C Grade Count:3 |
Overview of materials for Polypropylene w/ 50% Calcium Carbonate This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene w/ 50% Calcium Carbonate". Specific grades with calcium carbonate content between 45% and .. |