Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 95.4 µm/m-°C @Temperature 30.0 - 100 °C |
53.0 µin/in-°F @Temperature 86.0 - 212 °F |
ASTM E831 |
3M Dyneon™ CC085 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of PPS and other proprietary fillers blended with PTFE.Information provided by Dyneon, A 3M Company |