Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.10 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott LF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.10 µm/m-°C @Temperature 20.0 - 300 °C |
5.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-F2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.10 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.10 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott VG6 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 9.10 µm/m-°C @Temperature 20.0 - 300 °C |
5.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.10 µm/m-°C @Temperature 30.0 - 150 °C |
5.06 µin/in-°F @Temperature 86.0 - 302 °F |
|
Ametek Molybdenum-Copper Composite AMC 6436 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
CTE, linear | 9.10 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott GG395 Long Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG385, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630.. |