Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.8 µm/m-°C @Temperature 30.0 - 200 °C |
7.10 µin/in-°F @Temperature 86.0 - 392 °F |
|
International Mold Steel PX5 Pre-Hardened Mold Steel (P20 Type) PX5 is a modified P20, high performance, high precision, mold steel. Unique Characteristics: Exceptionally clean steel with uniform microstructure – no pin holes, inclusions or hard spots. 30-3.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.0 - 93.0 °C |
7.10 µin/in-°F @Temperature 69.8 - 199 °F |
|
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 302 °C |
7.10 µin/in-°F @Temperature 70.0 - 575 °F |
|
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel Description: P-20 High Hard is an improved pre-hardened mold steel that has been specially designed for large plastic molds; Material is forged on a 5000 ton press assuring maximum deformation durin.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 302 °C |
7.10 µin/in-°F @Temperature 70.0 - 575 °F |
|
Schmolz + Bickenbach P-20 Modified Plastic Mold Steel Description: P-20 Modified is an improved pre-hardened mold steel that has been specially designed for large plastic molds; The material is forged on a 5000 ton press assuring maximum deformation du.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 399 °C |
7.10 µin/in-°F @Temperature 70.0 - 750 °F |
|
Schmolz + Bickenbach Thermodur® E38K Hot Work Die Steel Description: Thermodur® E38K is an electro slag remelted (ESR) modified H-11 die steel, developed for hot working applications where maximum mechanical strength (toughness) properties are require.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 427 °C |
7.10 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel CSM® 2 Mold Steel, AISI P20 CSM 2 is a prehardened, general purpose mold steel suitable for production of machined or EDM’d plastic mold and zinc die casting die components. CSM 2 is supplied prehardened at two hardnesses: re.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 316 °C |
7.10 µin/in-°F @Temperature 70.0 - 600 °F |
|
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 538 °C |
7.10 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11 Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 427 °C |
7.10 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel HALGRAPH® Tool Steel, AISI O6 Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 204 °C |
7.10 µin/in-°F @Temperature 70.0 - 400 °F |
|
Crucible Steel Nitriding #135 Modified Steel, AISI 4140 Modified Nitriding #135 steel is a modification of AISI 4140 specifically designed to be nitrided for high surface hardness and abrasion resistance.Information provided by Crucible Industries |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 538 °C |
7.10 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature -34.4 - 93.3 °C |
7.10 µin/in-°F @Temperature -30.0 - 200 °F |
parallel to lengthwise filaments; ASTM D696-42T |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature -34.4 - 93.3 °C |
7.10 µin/in-°F @Temperature -30.0 - 200 °F |
parallel to crosswise filaments; ASTM D696-42T |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
CTE, linear | 12.8 µm/m-°C @Temperature 21.1 - 399 °C |
7.10 µin/in-°F @Temperature 70.0 - 750 °F |
|
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength.. |