Polymer Property : CTE, linear = 6.20 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 300 °C
3.44 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck HPM 1700 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 300 °C
3.44 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck HPM 1701 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 100 °C
3.44 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck MoCu 85/15 Molybdenum-Copper Composite Material
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t..
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 300 °C
3.44 µin/in-°F

@Temperature 68.0 - 572 °F
Schott KG4 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG3, KG1, KG5
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 300 °C
3.44 µin/in-°F

@Temperature 68.0 - 572 °F
Schott KG5 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include KG2, KG3, KG4, KG1
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 300 °C
3.44 µin/in-°F

@Temperature 68.0 - 572 °F
Schott KZFS12 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.20 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.44 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-BAF10 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.20 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.44 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LASF41 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.20 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.44 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LASF44 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.20 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.44 µin/in-°F

@Temperature -22.0 - 158 °F
Schott P-SF67 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 1000 °C
3.44 µin/in-°F

@Temperature 68.0 - 1830 °F
ASTM-C372
CeramTec Rubalit® 600 Alumina, 48%
Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors.
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 300 °C
3.44 µin/in-°F

@Temperature 68.0 - 572 °F
ASTM-C372
CeramTec Rubalit® 702 Alumina, 85%
Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl..