Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 55.0 µm/m-°C @Temperature <=143 °C |
30.6 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature <=143 °C |
30.6 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature <=143 °C |
30.6 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature <=143 °C |
30.6 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature <=143 °C |
30.6 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature <=152 °C |
30.6 µin/in-°F @Temperature <=306 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature <=162 °C |
30.6 µin/in-°F @Temperature <=324 °F |
Average below Tg; ISO 11359 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 23.0 °C |
30.6 µin/in-°F @Temperature 73.4 °F |
MD; ASTM D696 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 200 °C |
30.6 µin/in-°F @Temperature 392 °F |
MD; ASTM D696 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 30.0 - 100 °C |
30.6 µin/in-°F @Temperature 86.0 - 212 °F |
ASTM E831 |
3M Dyneon™ CC503 PTFE, 15% Mineral Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings - FDA compliant, valve seats, seals.Data provided by Dyneon. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature -80.0 - 70.0 °C |
30.6 µin/in-°F @Temperature -112 - 158 °F |
ASTM D686-79 |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
CTE, linear | 55.0 µm/m-°C @Temperature -80.0 - 70.0 °C |
30.6 µin/in-°F @Temperature -112 - 158 °F |
ASTM D686-79 |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 23.0 - 100 °C |
30.6 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murpec® Polyetheretherketone In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature <=143 °C |
30.6 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature <=143 °C |
30.6 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |