Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 39.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 39.0 µm/m-°C

@Temperature <=58.0 °C
21.7 µin/in-°F

@Temperature <=136 °F
below Tg
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
CTE, linear 39.0 µm/m-°C

@Temperature -55.0 - 288 °C
21.7 µin/in-°F

@Temperature -67.0 - 550 °F
Z-Direction; ASTM D3386
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave
Features & Benefits:High thermal conductivity - Improved dielectric heat dissipation, enabling lower operating temperatures for high power applicationsLow loss tangent - Excellent high frequency per..
CTE, linear 39.0 µm/m-°C

@Temperature 100 - 200 °C
21.7 µin/in-°F

@Temperature 212 - 392 °F
Axial; ASTM E831
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy
Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and..
CTE, linear 39.0 µm/m-°C

@Temperature <=55.0 °C
21.7 µin/in-°F

@Temperature <=131 °F
below Tg
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
CTE, linear 39.0 µm/m-°C

@Temperature 100 - 200 °C
21.7 µin/in-°F

@Temperature 212 - 392 °F
Axial; ASTM E831
Chevron Phillips Xtel® XK2240 Polyphenylene Sulfide Alloy  (discontinued **)
Natural Color Polyphenylene Sulfide AlloyXtel™ XK2240 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of tough..
Copyright © lookpolymers.com All Rights Reserved