Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 34.0 µm/m-°C @Temperature -55.0 - 288 °C |
18.9 µin/in-°F @Temperature -67.0 - 550 °F |
Z-Direction; ASTM D3386-94 |
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
CTE, linear | 34.0 µm/m-°C @Temperature -55.0 - 288 °C |
18.9 µin/in-°F @Temperature -67.0 - 550 °F |
Z-Direction; ASTM D3386-94 |
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
CTE, linear | 34.0 µm/m-°C @Temperature 0.000 - 100 °C |
18.9 µin/in-°F @Temperature 32.0 - 212 °F |
Y-Direction; 5°C/min; ASTM D3386 |
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi.. |
|||
CTE, linear | 34.0 µm/m-°C @Temperature 25.0 - 150 °C |
18.9 µin/in-°F @Temperature 77.0 - 302 °F |
ASTM TMA |
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
CTE, linear | 34.0 µm/m-°C @Temperature 0.000 - 100 °C |
18.9 µin/in-°F @Temperature 32.0 - 212 °F |
FD; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded
&nbs AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
CTE, linear | 34.0 µm/m-°C @Temperature 24.0 - 149 °C |
18.9 µin/in-°F @Temperature 75.2 - 300 °F |
ASTM E831-93 |
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
CTE, linear | 34.0 µm/m-°C @Temperature 0.000 - 100 °C |
18.9 µin/in-°F @Temperature 32.0 - 212 °F |
y direction; IPC TM-650 2.4.24 |
Arlon DiClad 880 PTFE/Woven Fiberglass Laminate Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch.. |