Polymer Property : CTE, linear = 16.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 28.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E831
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled  (discontinued **)
LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat..