Thermal Properties Metric English Comments
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, 1.6 mm sheet
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, 6.3-38.1 mm plate
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, aged 1000 hours at 316°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, aged 1000 hours at 982°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, all-weld metal, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, all-weld metal, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, mill annealed
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 26.0 - 760 °C
8.83 µin/in-°F

@Temperature 78.8 - 1400 °F
Haynes Ultimet® alloy, plate, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
CTE, linear 15.9 µm/m-°C

@Temperature 25.0 - 900 °C
8.83 µin/in-°F

@Temperature 77.0 - 1650 °F
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
CTE, linear 15.9 µm/m-°C

@Temperature 260 °C
8.83 µin/in-°F

@Temperature 500 °F
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel
INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybd..
CTE, linear 15.9 µm/m-°C

@Temperature 400 °C
8.83 µin/in-°F

@Temperature 752 °F
Special Metals INCOLOY® alloy 864
INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma..
CTE, linear 15.9 µm/m-°C

@Temperature 25.0 - 450 °C
8.84 µin/in-°F

@Temperature 77.0 - 842 °F
Carlson 20 Plus Alloy
Carlson C20 Plus is a super-austenitic alloy, developed to provide maximum resistance to corrosion by sulfuric acid. Nickel chromium, molybdenum and copper contribute to the excellent overall resist..
CTE, linear 15.9 µm/m-°C

@Temperature 20.0 - 100 °C
8.83 µin/in-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
CTE, linear 15.9 µm/m-°C

@Temperature 20.0 - 100 °C
8.83 µin/in-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum 310H Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
CTE, linear 15.9 µm/m-°C

@Temperature 20.0 - 100 °C
8.83 µin/in-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum 310S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
CTE, linear 15.9 µm/m-°C

@Temperature 20.0 - 100 °C
8.83 µin/in-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Copyright © lookpolymers.com All Rights Reserved