Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 22.0 µm/m-°C @Temperature 0.000 - 100 °C |
12.2 µin/in-°F @Temperature 32.0 - 212 °F |
X-Direction; IPC-TM-650 2.4.41 |
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
12.2 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ASTM E831 |
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
12.2 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ASTM E831 |
Chevron Phillips Xtel® XK2240 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2240 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of tough.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
In machine direction. |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |