Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.8 µm/m-°C @Temperature 900 °C |
6.00 µin/in-°F @Temperature 1650 °F |
|
Plansee CFY Chromium-Iron-Yttrium The most typical use for CFY is as interconnects in fuel cells.Characteristics: Coefficient of expansion - designed for compatibility with that of the electrolyte in fuel cells Corrosion resistance.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 20.0 - 200 °C |
6.00 µin/in-°F @Temperature 68.0 - 392 °F |
|
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 25.0 - 100 °C |
6.00 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 25.0 - 100 °C |
6.00 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 25.0 - 100 °C |
6.00 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 20.0 - 204 °C |
6.00 µin/in-°F @Temperature 68.0 - 399 °F |
|
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 20.0 - 204 °C |
6.00 µin/in-°F @Temperature 68.0 - 399 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.00 µin/in-°F @Temperature 70.0 - 200 °F |
A and H900 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.00 µin/in-°F @Temperature 70.0 - 200 °F |
A and H900 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.00 µin/in-°F @Temperature 70.0 - 200 °F |
A and H900 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 0.000 - 316 °C |
6.00 µin/in-°F @Temperature 32.0 - 600 °F |
|
Crucible Steel 420 and 420F Chromium Steel Crucible 416 Plus is a hardenable chromium steel which is the general purpose cutlery grade. This grade is magnetic in all conditions. Information provided by Crucible Specialty Metals. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature -17.8 - 316 °C |
6.00 µin/in-°F @Temperature 0.000 - 600 °F |
|
Crucible Steel 440A Chromium Steel Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 26.7 - 538 °C |
6.00 µin/in-°F @Temperature 80.0 - 1000 °F |
|
Crucible Steel 440B Chromium Steel Crucible 440B Is a hardenable chromium steel which is cutlery grade having high attainable hardness and toughness. This grade is magnetic at all times. Information provided by Crucible Specialty Me.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 20.0 - 200 °C |
6.00 µin/in-°F @Temperature 68.0 - 392 °F |
|
Crucible Steel CPM® Rex® 76®(HS), AISI M48 High Speed Steel Rex® 76®(HS) CPM Rex 76 is a super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It is heat treatable to HRC 68-70. Its high carbon, vanadium and cobalt contents provide abrasion resis.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 0.000 - 320 °C |
6.00 µin/in-°F @Temperature 32.0 - 608 °F |
|
Crucible Steel CSM® 420 XL Stainless Steel CSM 420 XL is the workhorse premium quality stainless mold steel designed for applications requiring a combination of corrosion resistance and wear resistance. It is double melted for the microstruc.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 300 °C |
6.00 µin/in-°F @Temperature 572 °F |
|
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 21.0 - 93.0 °C |
6.00 µin/in-°F @Temperature 69.8 - 199 °F |
|
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 0.000 - 100 °C |
6.00 µin/in-°F @Temperature 32.0 - 212 °F |
|
AK Steel 410S Ferritic Stainless steel AK Steel 410S Stainless Steel is a non-hardening modification of Type 410. A small titanium addition minimizes austenite formation at high temperatures, thereby restricting the alloy's ability to h.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 24.0 - 260 °C |
6.00 µin/in-°F @Temperature 75.2 - 500 °F |
|
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 468°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 20.0 - 400 °C |
6.00 µin/in-°F @Temperature 68.0 - 752 °F |
|
Assab Steels ASSAB XW-5 Cold Work Steel ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 20.0 - 260 °C |
6.00 µin/in-°F @Temperature 68.0 - 500 °F |
|
ATI Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed AL 433™ is a stainless steel in the ferritic family of alloys with Type 409 and Type 439. The AL 433 alloy contains 20% chromium for pitting and crevice corrosion resistance in the presence of chl.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 20.0 - 700 °C |
6.00 µin/in-°F @Temperature 68.0 - 1290 °F |
|
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 20.0 - 700 °C |
6.00 µin/in-°F @Temperature 68.0 - 1290 °F |
|
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy Allegheny Ludlum stainless Type AL 441HP™ alloy is a heat resisting ferritic grade providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dua.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 24.0 - 260 °C |
6.00 µin/in-°F @Temperature 75.2 - 500 °F |
|
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.00 µin/in-°F @Temperature 75.2 - 199 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.00 µin/in-°F @Temperature 75.2 - 199 °F |
H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 21.0 - 93.0 °C |
6.00 µin/in-°F @Temperature 69.8 - 199 °F |
|
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 25.0 - 100 °C |
6.00 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 0.000 - 100 °C |
6.00 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corrosio.. |
|||
CTE, linear | 10.8 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.00 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock a.. |