Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.62 µm/m-°C @Temperature 25.0 - 260 °C |
5.900 µin/in-°F @Temperature 77.0 - 500 °F |
|
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Longitudinal Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |
|||
CTE, linear | 10.62 µm/m-°C @Temperature 25.0 - 260 °C |
5.900 µin/in-°F @Temperature 77.0 - 500 °F |
|
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Transverse Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |
|||
CTE, linear | 10.62 µm/m-°C @Temperature 25.0 - 260 °C |
5.900 µin/in-°F @Temperature 77.0 - 500 °F |
|
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Longitudinal Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |
|||
CTE, linear | 10.62 µm/m-°C @Temperature 25.0 - 260 °C |
5.900 µin/in-°F @Temperature 77.0 - 500 °F |
|
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Transverse Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |