Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 177 µm/m-°C @Temperature -30.0 - 30.0 °C |
98.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp YF005 LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 177 µm/m-°C @Temperature -30.0 - 30.0 °C |
98.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP YF005 POLYESTER ELASTOMER LNP* THERMOCOMP* YF005 is a compound based on Polyester Elastomer resin containing 25% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 177 µm/m-°C @Temperature 20.0 °C |
98.3 µin/in-°F @Temperature 68.0 °F |
|
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Transverse to Flow | 177 µm/m-°C @Temperature 20.0 °C |
98.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® LT 6040IH Nylon (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
CTE, linear, Transverse to Flow | 177 µm/m-°C @Temperature 0.000 - 100 °C |
98.3 µin/in-°F @Temperature 32.0 - 212 °F |
z direction; IPC TM-650 2.4.24 |
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi.. |
|||
CTE, linear, Transverse to Flow | 177 µm/m-°C @Temperature 20.0 °C |
98.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® LT 6040ISH Nylon (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
CTE, linear, Transverse to Flow | 177 µm/m-°C @Temperature 20.0 °C |
98.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® LT 6040 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |