Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature 20.0 °C |
53.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall Information Provided by LG Chem |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature 20.0 °C |
53.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical HT-700 ABS, High Strength, High Scratch Resistance Information Provided by LG Chem |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature 20.0 °C |
53.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical LG-749 ABS, Low Gloss, High Heat Resistance Information Provided by LG Chem |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature 20.0 °C |
53.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical SH-610 ABS, Extrusion, High Impact Information Provided by LG Chem |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
53.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP IN001 PA6.12 LNP* LUBRICOMP* IN001 is a compound based on Nylon 6/12 resin containing 2% Moly. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
53.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFL46 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL46 is a compound based on PA66 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
53.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp QF002 PA6.10 LNP* Thermocomp* QF002 is a compound based on Nylon 6/10 containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C | 53.3 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
53.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam MX06089 PP, Flame Retardant, Injection Molding Starflam MX06089 is an Unfilled Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C | 53.3 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
53.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
53.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East) LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing Glass Fiber |
|||
CTE, linear, Transverse to Flow | 96.0 - 140 µm/m-°C | 53.3 - 77.8 µin/in-°F | Average value: 116 µm/m-°C Grade Count:4 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear, Transverse to Flow | 96.0 - 96.0 µm/m-°C @Temperature 55.0 - 160 °C |
53.3 - 53.3 µin/in-°F @Temperature 131 - 320 °F |
Average value: 96.0 µm/m-°C Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
CTE, linear, Transverse to Flow | 96.0 µm/m-°C @Temperature 20.0 °C |
53.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical HF-380 ABS, High Flow, High Impact Feature: Injection Molding, High FlowApplication: Electric & Electronic Products, Toys, Miscellaneous Goods)CAS No. 9003-56-9Information Provided by LG Chem |