Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
CTE, linear, Transverse to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
CTE, linear, Transverse to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
CTE, linear, Transverse to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
CTE, linear, Transverse to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
CTE, linear, Transverse to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl N190HX PPE+PS High gloss. 182F (83C) HDT. UL94 V-0/5VA rated.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |