Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 9.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
5.00 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66 LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |