Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 58.0 - 75.0 µm/m-°C | 32.2 - 41.7 µin/in-°F | Average value: 66.1 µm/m-°C Grade Count:8 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |