Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 131 µm/m-°C

@Temperature 20.0 °C
72.8 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 371A-12 CAP Cellulose Acetate Propionate  (discontinued **)
12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Transverse to Flow 131 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
CTE, linear, Transverse to Flow 131 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East)
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
CTE, linear, Transverse to Flow 131 µm/m-°C

@Temperature 23.0 - 60.0 °C
72.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT (Europe-Africa-Middle East)
LNP* LUBRICOMP* WI001 is a compound based on Polybutylene Terephalate resin containing Silicone. Added features include; Inernally Lubricated.
CTE, linear, Transverse to Flow 131 µm/m-°C

@Temperature 23.0 - 60.0 °C
72.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RF203 PA 66 (Europe-Africa-Middle East)
LNP* LUBRILOY* RF203 is a compound based on PA 66 resin containing Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.
CTE, linear, Transverse to Flow 131 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific)
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
CTE, linear, Transverse to Flow 131 µm/m-°C

@Temperature -30.0 - 30.0 °C
72.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-LOY M3000C PP
LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat.