Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature -30.0 - 30.0 °C |
69.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12 LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 23.0 - 60.0 °C |
69.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KL003E POM (Europe-Africa-Middle East) LNP* LUBRICOMP* KL003E is a compound based on Acetal Copolymer resin containing PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 23.0 - 60.0 °C |
69.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp MX96070 PP (Europe-Africa-Middle East) LNP* STARFLAM* MX96070 is a compound based on Polypropylene resin containing Flame Retardant. Added features include: Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 23.0 - 60.0 °C |
69.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MC004 PP (Europe-Africa-Middle East) LNP* Thermocomp* MC004 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 23.0 - 60.0 °C |
69.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MFB82I PP (Europe-Africa-Middle East) LNP* Thermotuf* MFB82I is a compound based on Polypropylene resin containing Glass Fiber, Glass Bead. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C | 69.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LM-05 HX nat PA12 Product description: Grilamid LM-05 HX natural is a medium viscosity, heat-stabilized nanocomposite PA12 extrusion and injection molding grade. The special features of Grilamid LM-05 HX natural are:.. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 55.0 - 160 °C |
69.4 µin/in-°F @Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m.. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 23.0 - 60.0 °C |
69.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C | 69.4 µin/in-°F | z direction |
Arlon AD300A Glass, PTFE and Micro-Dispersed Ceramic Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature -30.0 - 100 °C |
69.4 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications... |