Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® ULS-12LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An ultra low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices such as TSOPs and.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP AF006 ABS (Europe-Africa-Middle East) LNP* Thermocomp* AF006 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Europe-Africa-Middle East) NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RX02059 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX02059 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include; Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Apec® 1797 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 1881 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 2556 Polycarbonate MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 3158 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 3206 Polycarbonate ISO 7391-PC,M,(,,)-05-9MVR (300 °C/1.2 kg) 4.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable in transpar.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 6255 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 9415(Z) Polycarbonate Medium viscosity, flame retardant extrusion and injection molding grade with 10% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer Materia.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® AL2447 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® LED2045 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeMVR (250 °C/2.16 kg) 16.5 cm3/10minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable .. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® LTG2623 Polycarbonate PreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-X07208 PA410-I-GF30 % Glass Reinforced, Impact Modified |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® Rx2430 Polycarbonate ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 an.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® Rx2435 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® SF810 Polycarbonate, Glass Fiber Reinforced Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Structural foam• 10%.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT XE 3996 PA*-GF30 Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designatio.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |