Polymer Property : CTE, linear, Transverse to Flow = 64.6 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 64.6 µm/m-°C

@Temperature 20.0 °C
35.9 µin/in-°F

@Temperature 68.0 °F
ASTM E228
Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..
CTE, linear, Transverse to Flow 64.6 µm/m-°C

@Temperature -30.0 - 30.0 °C
35.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DFL36P PC
LNP* Lubricomp* DFL36P is a compound based on Polycarbonate containing 30% Glass Fiber 15% PTFE. Added features include: Exceptional Processing. Internally Lubricated.