Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 113 µm/m-°C

@Temperature 23.0 - 60.0 °C
62.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone.
CTE, linear, Transverse to Flow 113 µm/m-°C

@Temperature -30.0 - 30.0 °C
62.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66
LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant.
CTE, linear, Transverse to Flow 113 µm/m-°C

@Temperature -30.0 - 30.0 °C
62.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS
LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked.
CTE, linear, Transverse to Flow 113 µm/m-°C

@Temperature 23.0 - 60.0 °C
62.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT (Europe-Africa-Middle East)
LNP* Thermocomp* WF-1004 is a compound based on Polybutylene Terephalate resin containing Glass Fiber.
CTE, linear, Transverse to Flow 113 µm/m-°C
62.8 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612  (Unverified Data**)
33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 113 µm/m-°C
62.8 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers