Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 6.00 µm/m-°C | 3.33 µin/in-°F | Average value: 6.00 µm/m-°C Grade Count:6 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
CTE, linear, Transverse to Flow | 6.00 - 55.0 µm/m-°C | 3.33 - 30.6 µin/in-°F | Average value: 47.4 µm/m-°C Grade Count:38 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C @Temperature 25.0 - 1500 °C |
3.33 µin/in-°F @Temperature 77.0 - 2730 °F |
Perpendicular to pressing direction |
Momentive Performance Materials HBN Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
3.33 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66 LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C @Temperature 23.0 - 150 °C |
3.33 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 228 |
DuPont Performance Polymers VESPEL TP-8474 Polyimide DuPont Vespel TP-8474 parts are specified for mechanical, thermal, and tribological properties. TP-8474 parts offer excellent strength and toughness, dimensional stability, low outgassing, radiation.. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C | 3.33 µin/in-°F | DIN 53752 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C | 3.33 µin/in-°F | DIN 53752 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C | 3.33 µin/in-°F | DIN 53752 |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C | 3.33 µin/in-°F | Average value: 6.00 µm/m-°C Grade Count:6 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C | 3.33 µin/in-°F | DIN 53752 |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C | 3.33 µin/in-°F | DIN 53752 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Transverse to Flow | 6.00 µm/m-°C | 3.33 µin/in-°F | DIN 53752 |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |