Polymer Property : CTE, linear, Transverse to Flow = 59.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature -30.0 - 30.0 °C
59.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12
LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature -30.0 - 30.0 °C
59.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer
LNP LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing 15% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature 23.0 - 60.0 °C
59.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA6.10 (Europe-Africa-Middle East)
LNP*Lubricomp* QFL36 is a compound based on PA 6/10 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature 23.0 - 60.0 °C
59.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WL004 is a compound based on Polybutylene Terephalate resin containing PTFE.
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature -40.0 - 40.0 °C
59.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON CD0001 PS
LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature -40.0 - 40.0 °C
59.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON CD000I PS
LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature 23.0 - 60.0 °C
59.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KF004 Acetal Copolymer (Europe-Africa-Middle East)
LNP* THERMOCOMP* KF004 is a compound based on Acetal Copolymer containing Glass Fiber. Added features include : Chemically Coupled.
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature 23.0 - 60.0 °C
59.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East)
LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead.
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature -30.0 - 30.0 °C
59.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP WF0039U PBT
LNP* THERMOCOMP* WF0039U is a compound based on PBT resin containing 15% Glass Fiber. Added features of this grade include: Flame Retardant and UV Stabilized.
CTE, linear, Transverse to Flow 107 µm/m-°C
59.4 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
CTE, linear, Transverse to Flow 107 µm/m-°C
59.4 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6  (Unverified Data**)
30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym..