Polymer Property : CTE, linear, Transverse to Flow = 53.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 20.0 °C
53.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall
Information Provided by LG Chem
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 20.0 °C
53.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical HT-700 ABS, High Strength, High Scratch Resistance
Information Provided by LG Chem
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 20.0 °C
53.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical LG-749 ABS, Low Gloss, High Heat Resistance
Information Provided by LG Chem
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 20.0 °C
53.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical SH-610 ABS, Extrusion, High Impact
Information Provided by LG Chem
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
53.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP IN001 PA6.12
LNP* LUBRICOMP* IN001 is a compound based on Nylon 6/12 resin containing 2% Moly. Added feature of this grade is: Wear Resistant.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL46 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFL46 is a compound based on PA66 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
53.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp QF002 PA6.10
LNP* Thermocomp* QF002 is a compound based on Nylon 6/10 containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 96.0 µm/m-°C
53.3 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66  (Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam MX06089 PP, Flame Retardant, Injection Molding
Starflam MX06089 is an Unfilled Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 96.0 µm/m-°C
53.3 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/2
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East)
LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing Glass Fiber
CTE, linear, Transverse to Flow 96.0 - 140 µm/m-°C
53.3 - 77.8 µin/in-°F
Average value: 116 µm/m-°C Grade Count:4
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
CTE, linear, Transverse to Flow 96.0 - 96.0 µm/m-°C

@Temperature 55.0 - 160 °C
53.3 - 53.3 µin/in-°F

@Temperature 131 - 320 °F
Average value: 96.0 µm/m-°C Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 20.0 °C
53.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical HF-380 ABS, High Flow, High Impact
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products, Toys, Miscellaneous Goods)CAS No. 9003-56-9Information Provided by LG Chem