Polymer Property : CTE, linear, Transverse to Flow = 50.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
50.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Lubricomp KZL34 POM
LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas..
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY UX98388 PPA
LNP LUBRILOY* UX98388 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
50.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC
LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable.
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
50.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC
LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc..
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
50.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS
LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable.
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
50.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP NX10302 PC+ABS (Asia Pacific)
This is a PC/ABS compound with improved plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications.
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP PF005 PA 6 (Europe-Africa-Middle East)
25% glass fibre reinforced Polyamide 6 injection moulding resin.
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp RFC16 PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RFC16 is a compound based on PA 66 resin containing Glass Fiber, Carbon Fiber. Added features include: Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded
BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded
BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide RFC16 PA66/6, Glass/Carbon Fiber Filled, Injection Molded
RFC16 is a Glass Fiber and Carbon Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as STAR C PA66 C 303VY Z3)Information provided by Eurostar.